According to the cause of the bubble, the solution to the problem has the following aspects:
(1) When the wall thickness of the product is large, the cooling rate of the outer surface of the product is faster than that of the center portion. Therefore, as the cooling progresses, the resin edge of the center portion shrinks to expand toward the surface, causing insufficient filling of the center portion. This condition is called vacuum bubble. The main solutions are:

a) According to the wall thickness, determine the reasonable gate, runner size. The general gate height should be 50%~60% of the wall thickness of the product.

b) There is a certain amount of supplementary injection material until the gate is sealed.

C) The injection time should be slightly longer than the gate sealing time.

d) reduce the injection speed and increase the injection pressure,

e) Use a material with a high melt viscosity rating.

(2) As a result of the generation of volatile gas bubbles, the main solutions are:

a) Fully pre-dry.

b) Lower the temperature of the resin to avoid generating decomposition gases.

(3) Bubbles caused by poor fluidity can be solved by increasing the temperature of the resin and mold and increasing the injection speed.

According to the cause of the bubble, the solution to the problem has the following aspects:

(1) When the wall thickness of the product is large, the cooling rate of the outer surface of the product is faster than that of the center portion. Therefore, as the cooling progresses, the resin edge of the center portion shrinks to expand toward the surface, causing insufficient filling of the center portion. This condition is called vacuum bubble. The main solutions are:

a) According to the wall thickness, determine the reasonable gate, runner size. The general gate height should be 50%~60% of the wall thickness of the product.

b) There is a certain amount of supplementary injection material until the gate is sealed.

C) The injection time should be slightly longer than the gate sealing time.

d) reduce the injection speed and increase the injection pressure,

e) Use a material with a high melt viscosity rating.

(2) As a result of the generation of volatile gas bubbles, the main solutions are:

a) Fully pre-dry.

b) Lower the temperature of the resin to avoid generating decomposition gases.

(3) Bubbles caused by poor fluidity can be solved by increasing the temperature of the resin and mold and increasing the injection speed.


According to the cause of the bubble, the solution to the problem has the following aspects:

(1) When the wall thickness of the product is large, the cooling rate of the outer surface of the product is faster than that of the center portion. Therefore, as the cooling progresses, the resin edge of the center portion shrinks to expand toward the surface, causing insufficient filling of the center portion. This condition is called vacuum bubble. The main solutions are:

a) According to the wall thickness, determine the reasonable gate, runner size. The general gate height should be 50%~60% of the wall thickness of the product.

b) There is a certain amount of supplementary injection material until the gate is sealed.

C) The injection time should be slightly longer than the gate sealing time.

d) reduce the injection speed and increase the injection pressure,

e) Use a material with a high melt viscosity rating.

(2) As a result of the generation of volatile gas bubbles, the main solutions are:

a) Fully pre-dry.

b) Lower the temperature of the resin to avoid generating decomposition gases.

(3) Bubbles caused by poor fluidity can be solved by increasing the temperature of the resin and mold and increasing the injection speed.


お問い合わせ

Author:

Ms. He Lichun

Phone/WhatsApp:

+8613906114773

人気商品
企業ニュース
You may also like
Related Categories

この仕入先にメール

タイトル:
イーメール:
メッセージ:

Your message must be betwwen 20-8000 characters

お問い合わせ

Author:

Ms. He Lichun

Phone/WhatsApp:

+8613906114773

人気商品
企業ニュース

ホーム

Product

Phone

私たちに関しては

お問い合わせ

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

送信